Pipa Baja Karbon Mulus API 5L Gr. B/X42/X52/X65/ X70 Pls1 Psl2 Pipa Jalur
| Kelas | API 5L Kelas B, X42, X52, X56, X60, X65, X70, X80 |
| Tingkat Spésifikasi | PSL1, PSL2 |
| Rentang Diaméter Luar | 1/2” nepi ka 2”, 3”, 4”, 6”, 8”, 10”, 12”, 16 inci, 18 inci, 20 inci, 24 inci nepi ka 40 inci. |
| Jadwal Kandel | SCH 10. SCH 20, SCH 40, SCH STD, SCH 80, SCH XS, nepi ka SCH 160 |
| Jenis Manufaktur | Mulus (Digulung Panas sareng Digulung Tiis), Dilas ERW (Dilas Résistansi Listrik), SAW (Dilas Busur Terendam) dina LSAW, DSAW, SSAW, HSAW |
| Tipe Tungtung | Tungtung miring, Tungtung polos |
| Rentang Panjang | SRL (Panjang Acak Tunggal), DRL (Panjang Acak Ganda), 20 FT (6 méter), 40FT (12 méter) atanapi, khusus |
| Topi Protéksi | plastik atawa beusi |
| Perawatan Permukaan | Alami, Divernis, Lukisan Hideung, FBE, 3PE (3LPE), 3PP, CWC (Dilapis Beurat Beton) CRA Dilapis atanapi Dilapis |
Pipa API 5L nujul kana pipa baja karbon anu dianggo dina sistem transmisi minyak sareng gas. Pipa ieu ogé dianggo pikeun ngangkut cairan sanés sapertos uap, cai, sareng leutak.
Spésifikasi API 5L ngawengku jinis fabrikasi anu dilas sareng anu tanpa sambungan.
Jenis-jenis anu dilas: Pipa ERW, SAW, DSAW, LSAW, SSAW, HSAW
Jenis umum pipa las API 5L nyaéta sapertos kieu:
ERWLas résistansi listrik, biasana dianggo pikeun diaméter pipa anu kirang ti 24 inci.
DSAW/SAWLas busur terendam dua sisi/las busur terendam, metode las alternatif pikeun ERW anu dianggo pikeun pipa diaméter anu langkung ageung.
LSAWLas busur terendam longitudinal, dianggo pikeun diaméter pipa dugi ka 48 inci. Ogé katelah prosés fabrikasi JCOE.
SSAW/HSAW: Las busur terendam spiral/las busur terendam spiral, dianggo pikeun diaméter pipa dugi ka 100 inci.
Jenis Pipa Seamless: Pipa Seamless Hot-rolled sareng Pipa Seamless Cold-rolled
Pipa seamless biasana dianggo pikeun pipa diaméter leutik (biasana kirang ti 24 inci).
(Pipa baja seamless langkung umum dianggo tibatan pipa anu dilas pikeun diaméter pipa kirang ti 150 mm (6 inci).
Kami ogé nawiskeun pipa seamless diaméter ageung. Ngagunakeun prosés manufaktur hot-rolled, kami tiasa ngahasilkeun pipa seamless dugi ka 20 inci (508 mm) diaméterna. Upami anjeun peryogi pipa seamless anu diaméterna langkung ageung tibatan 20 inci, kami tiasa ngahasilkeunana nganggo prosés hot-expanded dugi ka 40 inci (1016 mm) diaméterna.
API 5L ngawengku Kelas B, X42, X46, X52, X56, X60, X65, X70, sareng X80.
Pipa baja API 5L ngagunakeun rupa-rupa tingkatan baja, kalebet Tingkatan B, X42, X46, X52, X56, X60, X65, X70, sareng X80. Nalika tingkatan baja ningkat, kontrol sarimbag karbon janten langkung ketat sareng sipat kakuatan mékanis janten langkung luhur.
Salian ti éta, komposisi kimia pipa seamless API 5L sareng pipa las tina kelas baja anu sami béda-béda, kalayan pipa las anu gaduh sarat anu langkung ketat sareng kandungan karbon sareng walirang anu langkung handap.
Komposisi Kimia pikeun pipa PSL 1 kalayan t ≤ 0,984” | |||||||
| Kelas Baja | Fraksi massa, % dumasar kana analisis panas sareng produk a,g | ||||||
| C | Mn | P | S | V | Nb | Ti | |
| maksimal b | maksimal b | maksimal | maksimal | maksimal | maksimal | maksimal | |
| Pipa Mulus | |||||||
| A | 0.22 | 0.9 | 0.03 | 0.03 | – | – | – |
| B | 0.28 | 1.2 | 0.03 | 0.03 | c,d | c,d | d |
| X42 | 0.28 | 1.3 | 0.03 | 0.03 | d | d | d |
| X46 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X52 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X56 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X60 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X65 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X70 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| Pipa anu dilas | |||||||
| A | 0.22 | 0.9 | 0.03 | 0.03 | – | – | – |
| B | 0.26 | 1.2 | 0.03 | 0.03 | c,d | c,d | d |
| X42 | 0.26 | 1.3 | 0.03 | 0.03 | d | d | d |
| X46 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X52 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X56 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X60 | 0.26 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X65 | 0.26 e | 1.45 e | 0.03 | 0.03 | f | f | f |
| X70 | 0.26e | 1.65 e | 0.03 | 0.03 | f | f | f |
| a. Cu ≤ = 0,50% Ni; ≤ 0,50%; Cr ≤ 0,50%; jeung Mo ≤ 0,15%, | |||||||
| b. Pikeun unggal réduksi 0,01% di handap konsentrasi maksimum anu ditangtukeun pikeun karbon, paningkatan 0,05% di luhur konsentrasi maksimum anu ditangtukeun pikeun Mn diidinan, dugi ka maksimum 1,65% pikeun kelas ≥ L245 atanapi B, tapi ≤ L360 atanapi X52; dugi ka maksimum 1,75% pikeun kelas > L360 atanapi X52, tapi < L485 atanapi X70; sareng dugi ka maksimum 2,00% pikeun kelas L485 atanapi X70., | |||||||
| c. Kajaba lamun aya kasapukan séjén NB + V ≤ 0,06%, | |||||||
| d. Nb + V + TI ≤ 0,15%, | |||||||
| e. Kajaba lamun aya kasapukan séjén., | |||||||
| f. Kajaba aya kasapukan séjén, NB + V = Ti ≤ 0,15%, | |||||||
| g. Teu aya panambahan B anu disengaja anu diidinan sareng sésa B ≤ 0,001% | |||||||
| Komposisi Kimia pikeun pipa PSL 2 kalayan t ≤ 0.984” | |||||||||||||||||||||
| Kelas Baja | Fraksi massa, % dumasar kana analisis panas sareng produk | Sarua jeung Karbon | |||||||||||||||||||
| C | Si | Mn | P | S | V | Nb | Ti | Anu sanésna | CE IIW | CE Pcm | |||||||||||
| maksimal b | maksimal | maksimal b | maksimal | maksimal | maksimal | maksimal | maksimal | maksimal | maksimal | ||||||||||||
| Pipa Mulus sareng Dilas | |||||||||||||||||||||
| BR | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | c | c | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42R | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | 0.06 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| BN | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | c | c | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42N | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | 0.06 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46N | 0.24 | 0.4 | 1.4 | 0.025 | 0.015 | 0.07 | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X52N | 0.24 | 0.45 | 1.4 | 0.025 | 0.015 | 0.1 | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X56N | 0.24 | 0.45 | 1.4 | 0.025 | 0.015 | 0.10f | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X60N | 0.24f | 0.45f | 1.40f | 0.025 | 0.015 | 0.10f | 0.05f | 0.04f | g,h,l | Sakumaha anu disatujuan | |||||||||||
| BQ | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42Q | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46Q | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X52Q | 0.18 | 0.45 | 1.5 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X56Q | 0.18 | 0.45f | 1.5 | 0.025 | 0.015 | 0.07 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X60Q | 0.18f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X65Q | 0.18f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X70Q | 0.18f | 0.45f | 1.80f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X80Q | 0.18f | 0.45f | 1.90f | 0.025 | 0.015 | g | g | g | i,j | Sakumaha anu disatujuan | |||||||||||
| X90Q | 0.16f | 0.45f | 1.9 | 0.02 | 0.01 | g | g | g | j,k | Sakumaha anu disatujuan | |||||||||||
| X100Q | 0.16f | 0.45f | 1.9 | 0.02 | 0.01 | g | g | g | j,k | Sakumaha anu disatujuan | |||||||||||
| Pipa anu dilas | |||||||||||||||||||||
| BM | 0.22 | 0.45 | 1.2 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42M | 0.22 | 0.45 | 1.3 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46M | 0.22 | 0.45 | 1.3 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X52M | 0.22 | 0.45 | 1.4 | 0.025 | 0.015 | d | d | d | e,l | 0.43 | 0.25 | ||||||||||
| X56M | 0.22 | 0.45f | 1.4 | 0.025 | 0.015 | d | d | d | e,l | 0.43 | 0.25 | ||||||||||
| X60M | 0.12f | 0.45f | 1.60f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X65M | 0.12f | 0.45f | 1.60f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X70M | 0.12f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X80M | 0.12f | 0.45f | 1.85f | 0.025 | 0.015 | g | g | g | i,j | .043f | 0.25 | ||||||||||
| X90M | 0.1 | 0.55f | 2.10f | 0.02 | 0.01 | g | g | g | i,j | – | 0.25 | ||||||||||
| X100M | 0.1 | 0.55f | 2.10f | 0.02 | 0.01 | g | g | g | i,j | – | 0.25 | ||||||||||
| a. SMLS t>0.787”, wates CE kedah sakumaha anu disatujuan. Wates CEIIW anu diterapkeun fi C > 0.12% sareng wates CEPcm diterapkeun upami C ≤ 0.12%, | |||||||||||||||||||||
| b. Pikeun unggal réduksi 0,01% di handap maksimum anu ditangtukeun pikeun C, paningkatan 0,05% di luhur maksimum anu ditangtukeun pikeun Mn diidinan, dugi ka maksimum 1,65% pikeun kelas ≥ L245 atanapi B, tapi ≤ L360 atanapi X52; dugi ka maksimum 1,75% pikeun kelas > L360 atanapi X52, tapi < L485 atanapi X70; dugi ka maksimum 2,00% pikeun kelas ≥ L485 atanapi X70, tapi ≤ L555 atanapi X80; sareng dugi ka maksimum 2,20% pikeun kelas > L555 atanapi X80., | |||||||||||||||||||||
| c. Kajaba lamun aya kasapukan séjén Nb = V ≤ 0,06%, | |||||||||||||||||||||
| d. Nb = V = Ti ≤ 0,15%, | |||||||||||||||||||||
| e. Iwal mun disebutkeun sapuk, Cu ≤ 0,50%; Ni ≤ 0,30% Cr ≤ 0,30% jeung Mo ≤ 0,15%, | |||||||||||||||||||||
| f. Kajaba lamun aya kasapukan séjén, | |||||||||||||||||||||
| g. Kajaba aya kasapukan séjén, Nb + V + Ti ≤ 0,15%, | |||||||||||||||||||||
| h. Iwal mun disebutkeun sapuk, Cu ≤ 0,50% Ni ≤ 0,50% Cr ≤ 0,50% jeung MO ≤ 0,50%, | |||||||||||||||||||||
| abdi. Iwal mun disebutkeun sapuk, Cu ≤ 0,50% Ni ≤ 1,00% Cr ≤ 0,50% jeung MO ≤ 0,50%, | |||||||||||||||||||||
| j. B ≤ 0,004%, | |||||||||||||||||||||
| k. Iwal mun disebutkeun sapuk, Cu ≤ 0,50% Ni ≤ 1,00% Cr ≤ 0,55% jeung MO ≤ 0,80%, | |||||||||||||||||||||
| l. Pikeun sadaya tingkatan pipa PSL 2 kecuali tingkatan anu aya catetan kaki j anu dicatet, hal ieu lumaku. Kajaba upami aya kasapukan sanés, teu aya tambahan B anu disengaja anu diidinan sareng sésa B ≤ 0,001%. | |||||||||||||||||||||
| PSL | Kaayaan Pangiriman | Kelas pipa |
| PSL1 | Digulung sakumaha anu dinormalisasi, dinormalisasi, dibentuk normalisasi | A |
| Digulung sakumaha anu digulung, dinormalisasi digulung, digulung termomékanis, dibentuk termomékanis, dibentuk normalisasi, dinormalisasi, dinormalisasi sareng ditemper atanapi upami disatujuan Q&T SMLS hungkul. | B | |
| Digulung sakumaha anu digulung, dinormalisasi digulung, digulung termomékanis, kabentuk termomékanis, kabentuk normalisasi, dinormalisasi, dinormalisasi sareng ditemper. | X42, X46, X52, X56, X60, X65, X70 | |
| PSL 2 | Digulung sakumaha anu digulung | BR, X42R |
| Normalisasi digulung, normalisasi dibentuk, dinormalisasi atanapi dinormalisasi sareng ditemper | BN, X42N, X46N, X52N, X56N, X60N | |
| Dipadamkeun sareng dipanaskeun | BQ, X42Q, X46Q, X56Q, X60Q, X65Q, X70Q, X80Q, X90Q, X100Q | |
| Digulung termomékanis atanapi dibentuk termomékanis | BM, X42M, X46M, X56M, X60M, X65M, X70M, X80M | |
| Digulung termomékanis | X90M, X100M, X120M | |
| Cukupna (R, N, Q atanapi M) pikeun kelas PSL2, kagolong kana kelas baja. |
PSL téh singgetan tina Product Specification Level, anu ngawengku PSL1 sareng PSL2. Éta ogé tiasa dihartikeun salaku tingkat kualitas.
PSL1 sareng PSL2 henteu ngan ukur béda dina sarat uji tapi ogé dina komposisi kimia sareng sipat mékanis.
PSL2 mibanda sarat anu langkung ketat tibatan PSL1 dina hal komposisi kimia, sipat tarik, uji dampak, uji non-destruktif, jsb.
Uji Dampak
PSL1 teu merlukeun uji dampak, sedengkeun PSL2 (kajaba X80) merlukeun uji dampak.
Uji Non-destruktif
PSL1 henteu meryogikeun uji coba non-destruktif, sedengkeun PSL2 meryogikeun.
(Uji non-destruktif: Uji non-destruktif sareng uji dina standar API 5L nganggo radiografi, ultrasonik, atanapi metode sanésna (tanpa ngancurkeun bahan) pikeun ngadeteksi cacad sareng ketidaksempurnaan dina pipa.)
Bungkusan nyaétaumumna taranjang, pangiket kawat baja, pisankuat.
Upami anjeun gaduh sarat khusus, anjeun tiasa nganggokemasan anti karat, jeung leuwih geulis.
Pancegahan pikeun kemasan sareng transportasi pipa baja karbon
1.Pipa Baja API 5Lkudu dijaga tina karusakan anu disababkeun ku tabrakan, ekstrusi, sareng potongan salami transportasi, panyimpenan, sareng panggunaan.
2. Nalika nganggo pipa baja karbon, anjeun kedah nuturkeun prosedur operasi kaamanan anu saluyu sareng merhatoskeun pikeun nyegah ledakan, kahuruan, karacunan sareng kacilakaan sanésna.
3. Salila dianggo,Pipa API 5L baja karbonkedah nyingkahan kontak sareng suhu anu luhur, média korosif, jsb. Upami dianggo dina lingkungan ieu, pipa baja karbon anu didamel tina bahan khusus sapertos tahan suhu anu luhur sareng tahan korosi kedah dipilih.
4. Nalika milih pipa baja karbon, pipa baja karbon tina bahan sareng spésifikasi anu cocog kedah dipilih dumasar kana pertimbangan anu komprehensif sapertos lingkungan panggunaan, sipat média, tekanan, suhu sareng faktor sanésna.
5. Sateuacan pipa baja karbon dianggo, pamariksaan sareng tés anu diperyogikeun kedah dilaksanakeun pikeun mastikeun yén kualitasna nyumponan sarat.
Transportasi:Pangiriman Ekspres (Pangiriman Sampel), Udara, Kareta Api, Darat, Pangiriman Laut (FCL atanapi LCL atanapi Massal)
Q: Naha produsén ua?
A: Sumuhun, kami produsén tabung baja spiral anu aya di désa Daqiuzhuang, kota Tianjin, Cina
Q: Dupi abdi tiasa mesen sababaraha ton kanggo uji coba?
A: Tangtosna. Kami tiasa ngirimkeun kargo kanggo anjeun nganggo layanan LCL. (Muatan kontainer kirang)
Q: Upami sampel gratis?
A: Sampel gratis, tapi anu mésér mayar ongkos kirimna.
Q: Naha anjeun supplier emas sareng ngalakukeun jaminan perdagangan?
A: Kami 13 taun supplier emas sareng nampi jaminan perdagangan.