Pipa Standar API 5L (Pipa API) – Pipa Seamless API 5L (Pipa Seamless API) tina Kelas Bahan API 5L: API 5L Gr B (API 5L B), API 5L Gr B PSL2, API 5L X42, API 5L X60 (Pipa X60), API 5L X65 (Pipa API 5L X65), API 5L X70 (Pipa X70), API 5L X80, sareng Pipa PSL2 & Pipa API Sch 40 | Patuh kana Standar Pipa API & Spésifikasi Pipa API
| Fitur | Spésifikasi |
| Kelas | API 5L B, X42, X52, X56, X60, X65, X70, X80 |
| Tingkat Spésifikasi | PSL1, PSL2 |
| Rentang Diaméter Luar | 1/2” – 40” (kalebet 2”, 3”, 4”, 6”, 8”, 10”, 12”, 16”, 18”, 20”, 24”) |
| Kandel Témbok (Jadwal) | SCH 10, 20, 40, STD, 80, XS, nepi ka 160 |
| Jenis Manufaktur | Mulus (digulung panas / digulung tiis), ERW (Dilas Résistansi Listrik), SAW (LSAW, DSAW, SSAW, HSAW) |
| Tungtung Pipa | Miring atanapi Polos |
| Pilihan Panjang | SRL (Acak Tunggal), DRL (Acak Ganda), 20FT (6m), 40FT (12m), atanapi disaluyukeun |
| Topi Protéksi | Plastik atanapi Beusi |
| Pilihan Perawatan / Pelapis Permukaan | Alami, Divernis, Lukisan Hideung, FBE, 3PE (3LPE), 3PP, CWC (Dilapis Beurat Beton), Dilapis atanapi Dilapis CRA |
Pipa API5L nyaéta tabung baja karbon anu dianggo dina angkutan minyak sareng gas. Pipa ieu ogé dianggo pikeun ngangkut cairan sanés sapertos uap, cai sareng leutak.
Spésifikasi API 5L ngawengku jinis fabrikasi anu dilas sareng anu tanpa sambungan.
| Tipe | Pedaran | Aplikasi / Diaméter Khas |
|---|---|---|
| ERW | Dilas Résistansi Listrik | Diaméter < 24 inci |
| DSAW / SAW | Dilas Busur Terendam Dua Sisi / Dilas Busur Terendam | Pipa diaméter anu langkung ageung, alternatif pikeun ERW |
| LSAW | Dilas Busur Terendam Longitudinal (prosés JCOE) | Diaméterna nepi ka 48 inci |
| SSAW / HSAW | Spiral Submerged Arc Las / Helical SAW | Diaméterna nepi ka 100 inci |
Jenis Pipa Seamless: Pipa Seamless Hot-rolled sareng Pipa Seamless Cold-rolled
Pipa seamless biasana dianggo pikeun pipa diaméterna leutik (biasana kirang ti 24 inci).
(Pipa baja seamless langkung umum dianggo tibatan pipa anu dilas pikeun diaméter pipa kirang ti 150 mm (6 inci).
Kami ogé nawiskeun pipa seamless diaméter ageung. Ngagunakeun prosés manufaktur hot-rolled, kami tiasa ngahasilkeun pipa seamless dugi ka 20 inci (508 mm) diaméterna. Upami anjeun peryogi pipa seamless anu diaméterna langkung ageung tibatan 20 inci, kami tiasa ngahasilkeunana nganggo prosés hot-expanded dugi ka 40 inci (1016 mm) diaméterna.
API 5L ngawengku Kelas B, X42, X46, X52, X56, X60, X65, X70, sareng X80.
Pipa baja API 5L ngagunakeun rupa-rupa tingkatan baja, kalebet Tingkatan B, X42, X46, X52, X56, X60, X65, X70, sareng X80. Nalika tingkatan baja ningkat, kontrol sarimbag karbon janten langkung ketat sareng sipat kakuatan mékanis janten langkung luhur.
Salian ti éta, komposisi kimia pipa seamless API 5L sareng pipa las tina kelas baja anu sami béda-béda, kalayan pipa las anu gaduh sarat anu langkung ketat sareng kandungan karbon sareng walirang anu langkung handap.
Komposisi Kimia pikeun pipa PSL 1 kalayan t ≤ 0,984” | |||||||
| Kelas Baja | Fraksi massa, % dumasar kana analisis panas sareng produk a,g | ||||||
| C | Mn | P | S | V | Nb | Ti | |
| maksimal b | maksimal b | maksimal | maksimal | maksimal | maksimal | maksimal | |
| Pipa Mulus | |||||||
| A | 0.22 | 0.9 | 0.03 | 0.03 | – | – | – |
| B | 0.28 | 1.2 | 0.03 | 0.03 | c,d | c,d | d |
| X42 | 0.28 | 1.3 | 0.03 | 0.03 | d | d | d |
| X46 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X52 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X56 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X60 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X65 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X70 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| Pipa anu dilas | |||||||
| A | 0.22 | 0.9 | 0.03 | 0.03 | – | – | – |
| B | 0.26 | 1.2 | 0.03 | 0.03 | c,d | c,d | d |
| X42 | 0.26 | 1.3 | 0.03 | 0.03 | d | d | d |
| X46 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X52 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X56 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X60 | 0.26 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X65 | 0.26 e | 1.45 e | 0.03 | 0.03 | f | f | f |
| X70 | 0.26e | 1.65 e | 0.03 | 0.03 | f | f | f |
| a. Cu ≤ = 0,50% Ni; ≤ 0,50%; Cr ≤ 0,50%; jeung Mo ≤ 0,15%, | |||||||
| b. Mn bisa ningkat 0,05% pikeun unggal réduksi 0,01% dina C, kalayan wates spésifik kelas 1,65%, 1,75%, sareng 2,00%. | |||||||
| c. Kajaba lamun aya kasapukan séjén NB + V ≤ 0,06%, | |||||||
| d. Nb + V + TI ≤ 0,15%, | |||||||
| e. Kajaba lamun aya kasapukan séjén., | |||||||
| f. Kajaba aya kasapukan séjén, NB + V = Ti ≤ 0,15%, | |||||||
| g. Teu aya panambahan B anu disengaja anu diidinan sareng sésa B ≤ 0,001% | |||||||
| Komposisi Kimia pikeun pipa PSL 2 kalayan t ≤ 0.984” | |||||||||||||||||||||
| Kelas Baja | Fraksi massa, % dumasar kana analisis panas sareng produk | Sarua jeung Karbon | |||||||||||||||||||
| C | Si | Mn | P | S | V | Nb | Ti | Anu sanésna | CE IIW | CE Pcm | |||||||||||
| maksimal b | maksimal | maksimal b | maksimal | maksimal | maksimal | maksimal | maksimal | maksimal | maksimal | ||||||||||||
| Pipa Mulus sareng Dilas | |||||||||||||||||||||
| BR | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | c | c | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42R | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | 0.06 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| BN | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | c | c | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42N | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | 0.06 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46N | 0.24 | 0.4 | 1.4 | 0.025 | 0.015 | 0.07 | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X52N | 0.24 | 0.45 | 1.4 | 0.025 | 0.015 | 0.1 | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X56N | 0.24 | 0.45 | 1.4 | 0.025 | 0.015 | 0.10f | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X60N | 0.24f | 0.45f | 1.40f | 0.025 | 0.015 | 0.10f | 0.05f | 0.04f | g,h,l | Sakumaha anu disatujuan | |||||||||||
| BQ | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42Q | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46Q | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X52Q | 0.18 | 0.45 | 1.5 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X56Q | 0.18 | 0.45f | 1.5 | 0.025 | 0.015 | 0.07 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X60Q | 0.18f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X65Q | 0.18f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X70Q | 0.18f | 0.45f | 1.80f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X80Q | 0.18f | 0.45f | 1.90f | 0.025 | 0.015 | g | g | g | i,j | Sakumaha anu disatujuan | |||||||||||
| X90Q | 0.16f | 0.45f | 1.9 | 0.02 | 0.01 | g | g | g | j,k | Sakumaha anu disatujuan | |||||||||||
| X100Q | 0.16f | 0.45f | 1.9 | 0.02 | 0.01 | g | g | g | j,k | Sakumaha anu disatujuan | |||||||||||
| Pipa anu dilas | |||||||||||||||||||||
| BM | 0.22 | 0.45 | 1.2 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42M | 0.22 | 0.45 | 1.3 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46M | 0.22 | 0.45 | 1.3 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X52M | 0.22 | 0.45 | 1.4 | 0.025 | 0.015 | d | d | d | e,l | 0.43 | 0.25 | ||||||||||
| X56M | 0.22 | 0.45f | 1.4 | 0.025 | 0.015 | d | d | d | e,l | 0.43 | 0.25 | ||||||||||
| X60M | 0.12f | 0.45f | 1.60f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X65M | 0.12f | 0.45f | 1.60f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X70M | 0.12f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X80M | 0.12f | 0.45f | 1.85f | 0.025 | 0.015 | g | g | g | i,j | .043f | 0.25 | ||||||||||
| X90M | 0.1 | 0.55f | 2.10f | 0.02 | 0.01 | g | g | g | i,j | – | 0.25 | ||||||||||
| X100M | 0.1 | 0.55f | 2.10f | 0.02 | 0.01 | g | g | g | i,j | – | 0.25 | ||||||||||
| a. SMLS t>0.787”, wates CE kedah sakumaha anu disatujuan. Wates CEIIW anu diterapkeun fi C > 0.12% sareng wates CEPcm diterapkeun upami C ≤ 0.12%, | |||||||||||||||||||||
| b. Mn bisa naék 0,05% pikeun unggal panurunan 0,01% dina C, kalayan wates luhur anu aya hubunganana sareng tingkat nyaéta 1,65%, 1,75%, 2,00% sareng 2,20%. | |||||||||||||||||||||
| c. Kajaba lamun aya kasapukan séjén Nb = V ≤ 0,06%, | |||||||||||||||||||||
| d. Nb = V = Ti ≤ 0,15%, | |||||||||||||||||||||
| e. Iwal mun disebutkeun sapuk, Cu ≤ 0,50%; Ni ≤ 0,30% Cr ≤ 0,30% jeung Mo ≤ 0,15%, | |||||||||||||||||||||
| f. Kajaba lamun aya kasapukan séjén, | |||||||||||||||||||||
| g. Kajaba aya kasapukan séjén, Nb + V + Ti ≤ 0,15%, | |||||||||||||||||||||
| h. Iwal mun disebutkeun sapuk, Cu ≤ 0,50% Ni ≤ 0,50% Cr ≤ 0,50% jeung MO ≤ 0,50%, | |||||||||||||||||||||
| abdi. Iwal mun disebutkeun sapuk, Cu ≤ 0,50% Ni ≤ 1,00% Cr ≤ 0,50% jeung MO ≤ 0,50%, | |||||||||||||||||||||
| j. B ≤ 0,004%, | |||||||||||||||||||||
| k. Iwal mun disebutkeun sapuk, Cu ≤ 0,50% Ni ≤ 1,00% Cr ≤ 0,55% jeung MO ≤ 0,80%, | |||||||||||||||||||||
| l. Pikeun sadaya tingkatan pipa PSL 2 kecuali tingkatan anu aya catetan kaki j anu dicatet, hal ieu lumaku. Kajaba upami aya kasapukan sanés, teu aya tambahan B anu disengaja anu diidinan sareng sésa B ≤ 0,001%. | |||||||||||||||||||||
PSL1
| Kaayaan Pangiriman | Kelas Pipa |
| Digulung sakumaha anu dinormalisasi, dinormalisasi, dibentuk normalisasi | A |
| Digulung sakumaha anu digulung, dinormalisasi digulung, digulung termomékanis, dibentuk termomékanis, dibentuk normalisasi, dinormalisasi, atanapi dinormalisasi & ditemper (atanapi Q&T SMLS upami sapuk) | B |
| Digulung sakumaha anu digulung, dinormalisasi digulung, digulung termomékanis, kabentuk termomékanis, kabentuk normalisasi, dinormalisasi, atanapi dinormalisasi & ditemper. | X42, X46, X52, X56, X60, X65, X70 |
PSL2
| Kaayaan Pangiriman | Kelas Pipa |
| Digulung sakumaha anu digulung | BR, X42R |
| Normalisasi digulung/dibentuk, dinormalisasi, atanapi dinormalisasi & ditemper | BN, X42N, X46N, X52N, X56N, X60N |
| Dipadamkeun & dipanaskeun | BQ, X42Q, X46Q, X56Q, X60Q, X65Q, X70Q, X80Q, X90Q, X100Q |
| Termomékanis digulung/dibentuk | BM, X42M, X46M, X56M, X60M, X65M, X70M, X80M |
| Gulungan termomékanis hungkul | X90M, X100M, X120M |
Catetan:Pikeun kelas PSL2, akhiran (R, N, Q, atanapi M) mangrupikeun bagian tina sebutan kelas baja.
PSL téh singgetan tina Product Specification Level, anu ngawengku PSL1 sareng PSL2. Éta ogé tiasa dihartikeun salaku tingkat kualitas.
PSL1 sareng PSL2 henteu ngan ukur béda dina sarat uji tapi ogé dina komposisi kimia sareng sipat mékanis.
PSL2 mibanda sarat anu langkung ketat tibatan PSL1 dina hal komposisi kimia, sipat tarik, uji dampak, uji non-destruktif, jsb.
Uji Dampak
PSL1 teu merlukeun uji dampak, sedengkeun PSL2 (kajaba X80) merlukeun uji dampak.
Uji Non-destruktif
PSL1 henteu meryogikeun uji coba non-destruktif, sedengkeun PSL2 meryogikeun.
(Pamariksaan pipa API 5L dilakukeun ku metode NDT sapertos radiografi, ultrasonik atanapi téknik NDT anu sanésna. Tés ieu tiasa mendakan cacad atanapi ketidaksempurnaan dina bahan pipa tanpa ngancurkeunana.)
Bungkusan
1. Inpormasi Bungkusan Bungkusan standar pipa polos kalayan tali kawat baja anu kandel.
2. Pilihan: anti karat sareng kemasan khusus pikeun ngajagi produk langkung saé sareng pikeun presentasi anu langkung saé.
Pancegahan Transportasi & Panganganan
1.Prost: ngalawan dampak, tekanan sareng motong salami transportasi, panyimpenan sareng penanganan.
2. Kasalametan: Anggo SOP pikeun bahan kimia pikeun ngaminimalkeun résiko kahuruan/ledakan/kontaminasi tfa.
3. Lingkungan gawé: Ulah kakeunaan suhu luhur, média korosif, atanapi lingkungan parah anu sanésna. Pipa anu didamel tina bahan suhu luhur, atanapi bahan tahan korosi pikeun aplikasi sapertos kitu.
4. Kriteria Pamilihan: Pamilihan bahan sareng kelas pipa kedah dilakukeun kalayan merhatoskeun lingkungan, média, tekanan sareng suhu sareng sarat proyék khusus.
5. Inspeksi Sateuacan Dianggo: Laksanakeun pamariksaan sareng tés anu diperyogikeun pikeun mastikeun yén kualitas sareng standar pipa parantos kacumponan.
Transportasi:Pangiriman Ekspres (Pangiriman Sampel), Udara, Kareta Api, Darat, Pangiriman Laut (FCL atanapi LCL atanapi Massal)
1. Naon bédana PSL1 sareng PSL2?
Sarat uji kimia, mékanis, sareng PSL2 langkung ketat tibatan PSL1, nawiskeun kualitas sareng reliabilitas anu unggul pikeun pipa kritis aset.
2. Naon waé tingkatan pipa?
Kelas anu sayogi nyaéta B, X42, X46, X5, X60, X65, X70, X80, X90. Sareng seueur deui kelas anu tiasa dihontal ngalangkungan kaayaan pangiriman anu béda-béda sapertos as-rolled, Normalized, Quenched & tempered atanapi Thermomechanically rolled.
3. Naon waé jinis pipa anu anjeun gaduh?
Kami tiasa nyayogikeun pipa SEAMLESS (SMLS), ERW, LSAW, DSAW, SSAW, sareng HSAW numutkeun kabutuhan proyék anu béda-béda.
4. Lapisan sareng perawatan permukaan naon anu disayogikeun?
Pilihanana nyaéta Natural mill finish, dicét hideung, FBE, 3PE (3LPE), 3PP, CWC (Beurat Beton Dilapis), dilapis atanapi dilapis ku CRA.
5. Kumaha milih pipa kelas anu leres?
Pilih dumasar kana tekanan operasi, suhu, jinis média sareng lingkungan. Tim téknis kami sayogi kanggo masihan naséhat anu mangpaat.